The spa step appears to have some large cracks that have been repaired previously.
There are no voids in the grout at the tile at the beach entry beyond normal wear.
A 24 hour water holding test was performed for the main body of the pool and it was determined to NOT be loosing water BEYOND a rate that exceeds the seasonal evaporate rate, according to the local CIMIS weather station.
The upper pool has some faux rockery cracking that may have water loss issues possible.
Plaster and Chemical Attack:
Cementitious surface coatings are susceptible to chemically and pH aggressive swimming pool water or to any chemical that is capable of deteriorating the cementitious materials of a surface coating.
Swimming pool water that is not in Ideal Range of acceptable tolerance (or “balanced”) as in accordance with the ANSI/APSP Standards is considered to be detrimental to cementitious surface coatings.
Depending on the direction of the imbalance a coating can either be stained or etched. Often, both staining and etching are exhibited on the surface of a coating as the pool water fluctuates from one extreme to the other.
There are visible signs of salt crystallization, surface efflorescence, or cracks that are emitting efflorescence or salt deposits which are common to a coating in contact with a positive saturation index (+ LSI), or “scaling” condition.
If the water is capable of leaching cement compounds from within the surface coating, then that water is in a negative saturation index (LSI), or "aggressive" condition.
If care is not taken to ensure that the water of a swimming pool is kept in an Ideal Range that is considered by ANSI/APSP to be balanced, and further that a sufficient amount of carbonate alkalinity buffer is constantly present, then the cementitious surface coating should be considered susceptible to damage from that water and deterioration may result.
Water-soluble salts, acids, or ions such as sulfates, chlorides, and carbonates, can be transported into a cementitious surface coating and react with the cementitious compounds. The resulting chemical reaction between the cementitious compounds and these salts, acids, or ions, in the presence of water, can cause deterioration to the coating. Acidic water aggressively attacks and dissolves cementitious surface materials.
Water that is low in hardness, or soft water, can cause leaching of certain compounds of the cement, especially calcium hydroxide.